Ceramic Fiber Paper Production Line

Wet-laid paper manufacturing for thin, flexible high-temperature gasketing

Ceramic fiber paper is a thin, flexible sheet made by a wet-laid process closely analogous to conventional papermaking. Bulk fiber is dispersed in water with a small binder fraction, formed on a wire at very low basis weight, dewatered, dried and calendered. The result is a sheet that can be die-cut, folded and wrapped — the thinnest and most formable product in the ceramic fiber family.

It fills the gap that needled products cannot. Below roughly 3mm, needling becomes impractical and paper takes over. Typical uses are gasketing, expansion joint filling, wrap for irregular shapes and electrical or thermal insulation in tight clearances. Because the sheet is thin and low-mass, even a modest line covers a large area of finished product.

The two process parameters that decide quality are formation uniformity at very low basis weight and controlled shrinkage through the dryer. Formation defects show as thin spots and pinholes; uncontrolled shrinkage shows as curl and dimensional drift. Both are addressed in the forming head design and the dryer tension profile, which is where we concentrate the engineering.

Technical Specifications

Annual Capacity200 – 1,500 tons/year
Classification Temperature1260°C / 1350°C / 1430°C
Thickness Range0.5mm – 6mm
Roll WidthUp to 1200mm
Basis WeightApprox. 100 – 1200 g/m² (thickness dependent)
DensityApprox. 180 – 250 kg/m³
Forming MethodWet-laid on forming wire
Binder ContentLow, organic binder burned out in service
DryingMulti-cylinder or through-air dryer
FinishingCalendering, slitting, rewinding
Control SystemPLC + HMI with basis weight monitoring
Power Supply380V/50Hz/3Phase (customizable)
Request Quotation Ask Technical Questions

Process Flow

How a ceramic fiber paper production line runs from raw material to finished product

Ceramic Fiber Paper Production Line: Bulk Fiber Slurrying → Refining & Dispersion → Binder Dosing → Dilution & Screening → Wet-laid Forming on Wire → Dewatering & Vacuum → Multi-zone Drying → Calendering → Thickness Gauging → Slitting → Rewinding → Packaging

Key Equipment Included

Applications

Where the output of this line is used

High-Temperature Gasketing

Die-cut gaskets for furnace doors, flanges, manways and access panels.

Expansion Joint Filling

Compressible filler for expansion joints and irregular gaps in refractory linings.

Wrap & Barrier Layers

Thin wrap insulation for tight clearances, electrical insulation and heat shields.

Why This Line From Jinyuan

Engineering decisions that show up in your daily operating cost

Formation held at low basis weight

The forming head and dilution system are designed for uniform sheet at 0.5mm, which is where thin spots and pinholes originate on under-specified lines.

Dryer tension profile controlled by zone

Independent zone tension prevents the curl and dimensional drift that come from drying a thin sheet too fast at the wet end.

White water closed-loop

Process water is recovered, screened and returned, which matters more on paper than any other ceramic fiber line because of the water-to-fiber ratio.

Frequently Asked Questions

Common questions before ordering a ceramic fiber paper production line

What thickness range can one line produce?
Standard configurations span about 0.5mm to 6mm. The practical limits are the forming head's dilution capability at the thin end and dryer capacity at the thick end. If your product list clusters at one end, we size the line for it rather than spreading across the full range.
What fiber grade is required?
Paper requires low-shot spun fiber. Shot particles cause pinholes and surface defects in a thin sheet. If you are producing your own feedstock on a cotton line, the fiberising route needs to be specified accordingly.
How does paper differ from felt?
Paper is wet-laid from slurry and is thin, dense and smooth — it die-cuts cleanly. Felt is needled, thicker, softer and more porous. Below about 3mm, paper is the practical choice; above it, felt is usually more economical.
What binder is used and what happens to it in service?
A small fraction of organic binder gives the sheet green strength for handling. It burns out during first heat-up, typically with a brief odour and fume release, which is normal and should be ventilated. Inorganic binder options exist for applications where burn-out is unacceptable.
Is the process water system complicated?
A wet-laid line moves a lot of water relative to fiber, so white water recovery is not optional — it is integral. The recovery and screening loop is included in the standard scope.

Related Equipment

Other production lines we build

Further Reading

Technical guides and buyer resources

Interested in This Production Line?

Send us your capacity requirement and product specifications for a tailored proposal.

Get a Free Quote