A changeover is not a re-threading. Re-threading restores a machine to the settings it was already running; a changeover changes the settings, and on a braiding line the settings that have to move are the ones that were coupled in the first place. That is why a changeover that only reloads yarn tends to produce a braid that looks right at the start of the roll and is wrong by the end of it.
This article separates the two kinds of changeover, lists what actually changes between them, gives the sequence in the order that avoids re-work, and covers the two things that decide whether the next changeover is shorter than this one: first-off approval and the parameter record.
Two Kinds of Changeover
Most changeovers are the smaller kind and should be treated as such. Changing to a new yarn lot of the same specification, same tex, same ply, on the same product, is a re-set: strip the carriers, load the new bobbins, thread to the same path, confirm the tension setting has not drifted, take a first-off sample. Nothing in the machine's geometry changes, and the parameter card stays valid.
The larger kind is a product change, and it is larger because it moves quantities that are coupled. A different section, a different interlacement, a different carrier count, or a different core and reinforcement material each change what the machine has to do — and because pitch, tension and lead are coupled to the product, at least one of them has to move with it.
What Actually Changes
| What is changing | What has to move with it | Why |
|---|---|---|
| Yarn specification — tex, ply or twist | Tension setting; pitch target; yarn consumption per metre | Tension was calibrated for the friction and stiffness of the previous yarn. A different yarn on the old setting arrives at the braiding point at the wrong tension, and the cover factor reached at a given pitch changes with the yarn's bulk. |
| Carrier count | Deck configuration; yarn ends to thread; pitch target | More carriers means more yarn ends per interlacement cycle, so the pitch that produced the approved cover factor on the old count over-closes on the new one. |
| Product diameter | Take-up setting — and therefore pitch and lead | Lead has to scale with the circumference to hold the braid angle constant. Running the new diameter on the old take-up reproduces the old pitch on a new circumference, which is a different braid angle. |
| Interlacement — 2×2 to 3×3 | Deck set-up; expected surface and section | Interlacement is a deck property, not a speed. Float length, crossover density and the visual standard for the finished braid all change with it. |
| Core or reinforcement material | Independent core tension; reinforcement feed phasing | 316L stainless steel wire and ECR glass fiber yarn are stiffer and less extensible than the ceramic yarn around them; run on the outer yarn's tension they dominate the section, run slack they carry nothing. |
| Bobbin format | Spindle seating checks | The bobbin has to match the spindle — the 336 series takes a φ70 × 165 mm bobbin — and be clamped, or pay-off wobble modulates the tension once per bobbin revolution. |
The rows in that table are drawn from our own changeover practice and from the process documentation the settings come from. (field practice)
The Sequence
The order matters because two of the steps destroy the work of others if taken out of turn.
- Isolate and decelerate. The machine is brought down to no-load before the drive is cut; an emergency stop under load damages machine parts and throws the yarn into a tangle that has to be re-threaded by hand. Doffing is only done with the power off — never from a running machine.
- Decide the machine state first. If the carrier count, interlacement or deck configuration is changing, that is done before any yarn is loaded. Loading bobbins and then discovering the deck has to change wastes the loading.
- Load bobbins. Three checks on each: bobbin size matched to the spindle, left centre pin engaged with the elastic pin, right centre aligned to the bore before the flange sleeve is turned back. Every carrier position, including the ones that will be empty — an unloaded position that should have been loaded leaves a soft spot in the braid, and every crossing around it is still correct, which is what makes the defect hard to see.
- Thread to the two rules. The path must not cross itself and must not bypass the tension drop-weight. The check is physical: follow the yarn from the package to the eyelet with a finger and confirm it lifts the weight.
- Set core and reinforcement tension independently of the outer yarn, and confirm the reinforcement enters at the braiding point in step with the outer yarn.
- Set pitch and haul-off last. The take-up is set after threading, not before, because the pitch target depends on the diameter and the construction that the first five steps have just established.
- Run the first-off sample and inspect it against the appearance requirements and the approved sample before the run is released.
- Complete the parameter record and keep it with the roll.
Why Re-Calibration Is Not Optional
Carrying a tension setting across a yarn change is the single most common changeover fault, and it fails quietly. The setting is a weight, and the weight was chosen to give the required tension on the previous yarn's path. Change the yarn's tex or twist and the same weight produces a different tension at the braiding point — sometimes only slightly different, which is worse, because the resulting braid passes a casual look and fails on coverage or on the tensile figure the customer tested.
The same argument applies to the take-up after a diameter change, and it is worth stating as a rule rather than a warning: whenever the product diameter changes, re-derive the take-up from the braid angle you need, do not inherit it. The relationship between the two is set out in the braid angle and pitch article in this series; the short version is that lead has to change in proportion to the circumference if the angle is to stay where the approved sample has it.
First-Off Approval
The first-off sample is what stops a changeover error from becoming a rejected delivery, and it is cheap — a metre of braid and ten minutes. Three things are checked, in this order: (field practice)
- Appearance against GB/T 3003-2006 — uniformly tight, smooth surface, closely packed pattern, no broken ends, no oil contamination; soft spots, exposed yarn ends, bends and dropped stitches each limited to three places within any continuous 10 m. (national standard)
- Pitch, measured over ten pattern repetitions and divided, not read off a single repeat. This is the number that catches a take-up left over from the previous product.
- Diameter and braid angle against the approved sample. A square diamond means the yarns cross at right angles; if the sample's diamond is square and the new roll's is not, the take-up is wrong for the new diameter even though the pitch looks plausible.
Only then is the run released. Releasing on appearance alone is what allows a whole roll to be produced at a pitch that fails cover factor — a fault that is invisible until the packing is installed and does not seal.
Carrier Count Is the Real Size of a Changeover
People ask how long a changeover takes, and the honest answer is that the clock time is not a property of the machine — it is a function of the configuration being changed to. The dominant drivers are the number of yarn ends that have to be seated and threaded, whether the deck or carrier count changes, and whether the yarn specification changes. A 64-carrier deck is 64 seats to check and 64 ends to thread to two routing rules, regardless of how fast anyone works; the same deck changing only the yarn lot is the same count of ends and none of the geometry.
That is also why the parameter record pays for itself. A changeover that leaves behind the settings that worked — carrier count, yarn specification, interlacement, tension setting, pitch and take-up, core and reinforcement material — turns the next changeover back to that product into a re-set rather than a re-derivation. Without the record, the next changeover starts from whatever the last operator remembers, and the settings that were coupled get inherited one at a time instead of moved as a set.
It is the same argument the braiding process article makes about every parameter on the line: a parameter without a recorded source is a parameter nobody can defend when a customer, an auditor or the next shift asks where it came from. (field practice)
Frequently Asked Questions
What actually changes in a braiding machine changeover?
It depends on whether the product changes. Changing to a new yarn lot of the same specification is a re-set: reload, re-thread, confirm the tension setting and take a first-off sample, with no change of machine geometry. A product change is larger because it moves coupled quantities. A yarn specification change moves tension and pitch; a carrier count change moves the deck configuration and the pitch target; a diameter change moves the take-up, and with it the lead and the braid angle; an interlacement change is a deck set-up; a core or reinforcement material change moves core tension and reinforcement phasing.
How long does a braiding machine changeover take?
There is no figure we would quote independent of the configuration, because clock time is not a property of the machine. The dominant drivers are the number of yarn ends to seat and thread, whether the deck or carrier count changes, and whether the yarn specification changes. A 64-carrier deck is 64 seats to check and 64 ends to thread to two routing rules; the same deck changing only the yarn lot is the same number of ends and none of the geometry. We would rather derive the figure from your configuration than publish a number that misleads.
Why re-calibrate yarn tension after changing the yarn?
Because the tension setting is a weight, and the weight was chosen to give the required tension on the previous yarn's path. Change the tex or the twist of the yarn and the same weight produces a different tension at the braiding point. The failure is quiet rather than obvious: a slightly wrong tension still produces a braid that passes a casual look, then fails on cover factor or on the tensile figure the customer tested. Re-calibration also covers the drop-weight path itself, which is checked physically by confirming the yarn actually lifts the weight.
What is first-off approval on a braiding line and what do you check?
First-off approval is inspecting the first metre of a new run before the run is released. Three things are checked, in order. Appearance against GB/T 3003-2006: uniformly tight, smooth surface, closely packed pattern, no broken ends or oil contamination, with soft spots, exposed yarn ends, bends and dropped stitches each limited to three places within any continuous 10 m. Pitch, measured over ten pattern repetitions and divided rather than read off one repeat, which catches a take-up inherited from the previous product. And diameter with braid angle against the approved sample — a square diamond means the yarns cross at right angles, so if the sample is square and the new roll is not, the take-up is wrong for the new diameter.
Can the carrier count be changed without changing the deck?
No — carrier count is a deck property. Carriers ride in slots cut into the horn gears on the deck plate and are handed from gear to gear as the teeth mesh, so the number of positions available is set by the gear train and the number of concentric tracks, not by a software setting. Changing the count therefore means a deck or configuration change, and because carrier count sets how many yarn ends enter each interlacement cycle, the pitch target has to be re-derived with it rather than inherited from the previous product.
What records should a changeover leave behind?
The settings that worked, written before the run and kept with the roll: carrier count, yarn specification, interlacement, tension setting, pitch and take-up, and the core and reinforcement material. Those are the quantities that move together, and recording them as a set is what turns the next changeover back to the same product into a re-set rather than a re-derivation. Without the record the next operator inherits the settings from memory and moves the coupled ones one at a time, which is how a braid ends up correct at one end of the roll and wrong at the other.