A ceramic fiber blanket is specified by where it will live. The same rolled product that backs a steel ladle lines a tunnel kiln car, seals a coke-oven door and wraps a turbine casing, and in each of those duties the thing that decides whether it survives is not the brand but three choices made on paper: the sector's working condition, the temperature grade that condition demands, and the physical form the geometry accepts. This page is the application map written as a specification document: five sectors with their working conditions, the temperature-to-grade-to-density ladder that selects the product, the form family from flat blanket to foil-faced composite, and the installation discipline that keeps a correct selection from failing in the field.
Our overview page lists where finished blankets go in five bullets and each product-line page carries a short applications section; what none of them holds is the working-condition detail behind each bullet, and that detail lives here. The grade names themselves — what separates standard from high-purity from high-alumina from zirconia in chemistry and classification temperature — are owned by our grade recipes page, and the test methods that prove a delivered roll meets its grade are on our testing page. This page assumes you already know the grade names and answers the question they leave open: which one, in which form, for which duty.
Metallurgy: The Backing That Lowers Shell Temperature
Metallurgy is the sector that taught the industry what a blanket is for. The duties cluster around one idea: a hot vessel with a steel shell that must stay cool enough to keep its strength, and a lining whose job is to put resistance between the two. A blanket or module backing behind a working refractory lining drops the shell temperature sharply, which is an energy saving and a shell-life saving at the same time; where the hot face is the blanket itself, the duty adds gas velocity and thermal shock to the temperature.
Metallurgical working conditions, the grade each demands and the form that fits
| Service condition | Grade | Form |
|---|---|---|
| Ladle, tundish backing | High-alumina, zirconia | Blanket, board |
| Blast-furnace hot-blast main | High-purity, high-alumina | Blanket, module |
| Coke-oven door seal | Standard, high-purity | Blanket, rope |
| Heating-furnace lining | High-alumina | Blanket, module |
Two rows in that table carry a lesson. The hot-blast main is a gas-velocity duty as much as a temperature duty, so it pairs blanket with module and asks for erosion resistance on top of grade; the coke-oven door is a sealing and thermal-shock duty where the door cycles open and closed, so a lower grade in a flexible form beats a higher grade in a rigid one. Reading the table as temperature alone is the common error; the form column is doing half the work.
Petrochemical: Where the Flue Gas Decides the Grade
Petrochemical duties add a second selector that metallurgy mostly lacks: chemistry in the gas stream. A cracking furnace lining sees hot, corrosive flue gas, which is why the zirconia grade appears here as the default rather than the exception; a reformer flue duct is a velocity duty in high-alumina; and the large population of valves, flanges and small fittings is a maintenance duty, where a removable blanket jacket wins precisely because it can be lifted off for inspection and put back. Heating and reforming furnaces take high-alumina blanket for the plain reason that every degree of shell temperature removed is fuel not burned.
The corrosion point deserves its own sentence because it reverses the usual selection logic. In a clean-air furnace the grade follows the temperature; in a corrosive flue the grade follows the gas, and a blanket rated comfortably for the temperature can still be consumed by the chemistry. Where the stream carries sulphur or alkali, specify one grade above what the thermometer asks for. What one grade above means in designation terms — and why the classification temperature on the label is never the service temperature in the lining — is read on our ceramic fiber grades page.
Power, Kilns and Waste: Three Demands, Three Different Answers
Power generation buys blanket for the boiler body, the turbine casing and the flue and air ducts, and it buys it for a reason beyond insulation: the material is Class A non-combustible, which satisfies fire codes that a combustible insulation cannot. Nuclear service is the same duty with a stricter purity and corrosion specification on top, and it is specified as such rather than assumed from a standard grade.
Building materials and ceramic kilns are the sector where the blanket's low heat storage is the product rather than a side benefit. Tunnel kiln cars, roller-kiln baffles and shuttle-kiln walls cycle hot and cold many times a day; a heavy lining stores heat on every ramp and gives it back on every cool-down, while a low-storage fiber lining lets the kiln change temperature fast. Published figures put the resulting energy saving in the 15-25 % band, and just as important, they let a kiln run the fast cycle its product mix now demands.
Environmental waste disposal — garbage incinerators and hazardous-waste kilns — is the harshest duty on the map. The temperature is high, but the deciding factor is the acid and alkali corrosion in the flue gas, which is why the zirconia grade is the first choice here rather than an upgrade reached for later.
The Selection Ladder: Temperature Sets Grade, Duty Sets Density
Compress the five sectors into one decision and it becomes a ladder of four rungs: the long-term service temperature selects the grade, and the mechanical duty selects the density. The table is the ladder as it is applied in practice; the densities are kilograms per cubic metre.
Service temperature selects the grade; the mechanical duty selects the density
| Long-term temperature | Grade | Density kg/m3 |
|---|---|---|
| Up to 1000 °C | Standard | 96-128 |
| Up to 1100 °C | High-purity | 96-128 |
| Up to 1200 °C | High-alumina | 128-160 |
| Up to 1300 °C | Zirconia | 128-160 |
| Erosion duty | High-alumina, zirconia | 160 |
| Curved, flexible fit | Standard, high-purity | 96-128 |
The last two rows are the duty corrections. An erosion duty — gas velocity, abrasion, a flame impinging — takes the top density and usually a surface coating on top of it, because density is what resists being scoured away. A duty that must wrap a curved surface takes the opposite move: a lower density with high rebound, because a stiff high-density blanket bridges a curve instead of following it. What each grade name means in chemistry and classification temperature is on our grade recipes page; how a delivered roll is proved against its grade, density and thickness is on our testing page, and the thickness-and-density pairing itself is argued on our thickness and density guide.
The Form Family: Blanket, Module, Folded Block, Foil-Faced, Shaped
Grade and density select the material; the form selects how it is delivered and held in place. Five forms cover essentially every duty on the map.
The five product forms and the duty each one wins
| Form | What it is | Where it wins |
|---|---|---|
| Flat blanket | Rolled, cut on site | General lining, pipes |
| Module | Pre-compressed, anchored | Furnace linings |
| Folded block | Blanket folded to block | Modular install |
| Foil-faced composite | Foil laminate, 95% reflect | Mid-low temp radiation |
| Shaped part | Custom geometry | Seals, gaskets, specials |
The module and the folded block are both answers to the same problem — a furnace lining that must stay on a hot wall without sagging — and they differ in how the compression is achieved and anchored, which is a fabrication and installation choice rather than a performance ranking. The foil-faced composite is the one form whose value is not conduction at all: an aluminium foil facing with a reflectance of 95 % or higher cuts radiant heat transfer, which is the dominant loss mechanism at mid and low temperature, so it earns its place on cabinets, ducts and pipework where a bare blanket would radiate straight through. Shaped parts are the remainder term: any geometry a roll cannot become, vacuum-formed to drawing. The rigid panel that shares this wet vacuum-forming route yet ships flat and load-bearing — the ceramic fiber board — is defined on our ceramic fiber board page.
Installation: Four Rules and One Warning
A correct selection fails in the field more often than on paper, and the failures are almost all installation failures. Four rules carry most of the discipline:
- Stagger the joints. Multi-layer work must be laid with offset joints; a through-seam in every layer is a thermal bridge straight to the shell, and it reads later as a hot spot nobody can explain.
- Respect the design compression. Module and folded-block products are made pre-compressed and must be installed to the design compression rate; under- or over-compression changes both the lining thickness and the load on the anchors.
- Match the anchor alloy to the temperature. A metal anchor is only as good as its oxidation resistance at service temperature; an anchor that oxidises away drops a perfectly good lining.
- Fill the seams with the same fiber. Joints are packed with same-material fiber and compacted, never left as gaps and never filled with a different product.
And the warning, stated plainly because it is the part of the application map nobody puts on a datasheet: cutting and laying blanket on site raises respirable fiber exposure far above what the production process produces, and public toxicology data — including the US NTP record — puts end-user exposure during installation above production-worker exposure. Installation crews need P2 or P100 respiratory protection, goggles and gloves, with wet cutting wherever the job allows it. The full exposure and control picture is on our safety page; the point here is only that the hazard belongs to the application, not just to the factory.
What We Deliberately Do Not Claim
Four boundaries. The sector tables and the selection ladder are the industry's common specification practice and our own application notes, not a quotation: actual grade, density and form for a given vessel are confirmed against the customer's operating data per project. The 15-25 % kiln energy-saving band and the foil reflectance figure are published industry values, cited as such. We publish no measured shell temperatures or saved-fuel figures from customer installations, because those belong to the customer and to their operating conditions. And we do not present any grade as universally correct: every row in every table here is a starting point that the duty, the gas chemistry and the geometry are entitled to overrule.
The Bottom Line
Ceramic fiber blanket reaches almost every industry that runs something hot, but it reaches them as five different products wearing one name: a metallurgical backing chosen for shell temperature, a petrochemical lining chosen for flue-gas chemistry, a power-plant insulation chosen for fire code, a kiln lining chosen for low heat storage, and a waste-disposal lining chosen for corrosion resistance. The ladder — temperature to grade, duty to density, geometry to form — is short enough to fit on one page and strict enough to prevent most field failures, and the four installation rules plus the exposure warning are what keep the paper decision true on the wall. Specify the duty first and the product follows; specify the product first and the duty will correct you later, at maintenance cost.
Frequently Asked Questions
Which industries use ceramic fiber blanket?
Essentially every industry that runs high temperature equipment: metallurgy for ladle and tundish backing, hot-blast mains and coke-oven door seals; petrochemical for cracker and reformer linings, flue ducts and removable valve jackets; power generation for boiler bodies, turbine casings and flue and air ducts; building materials and ceramics for tunnel kiln cars, roller-kiln baffles and shuttle-kiln walls; and environmental waste disposal for incinerators and hazardous-waste kilns. Outside those, fire protection wrapping, stress-relief insulation for welding and high-temperature gaskets take the same material in special forms.
What grade of ceramic fiber blanket suits 1200 degrees Celsius?
The high-alumina grade, at a density of 128 to 160 kilograms per cubic metre, is the standard answer for continuous service up to 1200 degrees Celsius, and it is also the grade chosen when thermal shock is part of the duty. If the gas stream is corrosive, or if the service temperature sits at the top of that band with little margin, the zirconia grade is the safer selection. The temperature in question should always be the long-term operating temperature, not a short peak, because grade ratings are continuous-service ratings.
What is the difference between a ceramic fiber module and a folded block?
Both are pre-compressed blanket delivered as a block for furnace linings, and both solve the same problem of holding a lining on a hot wall without sagging. They differ in how the compression is produced and how the block is anchored: a module is compressed and fitted with its anchor during manufacture, while a folded block is made by folding blanket to size and is anchored as part of installation. The choice is a fabrication and installation decision driven by the lining design, not a performance ranking between the two.
When should a foil-faced ceramic fiber blanket be used?
When the dominant heat loss is radiation rather than conduction, which is the case at mid and low temperature. An aluminium foil facing with a reflectance of 95 percent or higher reflects radiant heat back instead of letting it pass, so foil-faced composite earns its place on cabinets, ducts, pipework and enclosures where a bare blanket would radiate straight through. At furnace temperatures conduction and convection dominate and the foil adds little, so the facing is a mid-to-low temperature tool rather than a universal upgrade.
Why is ceramic fiber blanket used on tunnel kiln cars?
Because its heat storage is low. A kiln car cycles hot and cold many times a day, and a heavy brick lining stores heat on every ramp and returns it on every cool-down, wasting fuel and slowing the cycle. A low-storage fiber lining lets the car change temperature quickly, which is where the published 15 to 25 percent energy-saving band comes from, and it lets the kiln run the fast firing cycles that modern product mixes require. The same logic applies to roller-kiln baffles and shuttle-kiln walls.
Is installing ceramic fiber blanket more hazardous than producing it?
Yes, and this is the least-known fact on the application map. Cutting and laying blanket on site releases respirable fiber at concentrations far above those in the production process, and public toxicology records, including the US NTP data, put end-user exposure during installation above production-worker exposure. Installation crews therefore need P2 or P100 respiratory protection, goggles and gloves, with wet cutting wherever possible. The hazard belongs to the application stage, not only to the factory.